Rows of steel coils on pallets across the floor of a coil processing plant
buying-guide|Nov 20, 2026|11 min read

How to Specify Stainless Steel Interleaving Paper by Finish

#buying-guide#interleaving-paper

Request a Quote

Specify interleaving paper for stainless steel coils and sheets by finish first: 2R and polished finishes are limited by smoothness and dust, 2B by chloride, sulphate and moisture, and coil winding by tensile strength. Then give every limit a named test method; Table 3 is a template.

Key takeaways

  • Start from the process step and the EN 10088-2 finish, then decide which properties to specify most tightly.
  • Write pH as a range and chloride and sulphate as maximums in mg/kg, each with a named test method.
  • Bright and polished finishes need the smoothest, cleanest sheet; coil winding needs tensile strength.
  • Compare offers per square metre, not per tonne, when grammages differ.
Written forSteel mills, service centres and processors buying interleaving paper
Applications coveredCoil winding, slitting and cut sheets; 2B, 2R, 2J and 2K finishes
FormatsRolls to your coil widths, and cut sheets

What does interleaving paper do for stainless steel coils and sheets?

Interleaving paper keeps metal surfaces apart between coil wraps or stacked sheets, so they do not rub, mark or stick during winding, handling and transport. In steel mills and service centres it is part of the coil packaging: it protects the finish against abrasion when coils are wound and uncoiled, and helps prevent scratches when sheets slide over each other. It can also take up small amounts of residual oil or moisture. What it must not do is add anything to the surface: moisture, acidity, soluble salts, dust or loose fibre.

The paper is a separator, not a corrosion inhibitor. For parts that need inhibition inside a closed pack, see how to specify anti-rust paper for packed parts. Some processors use PE film instead of paper; the choice depends on the line, the finish and the end customer's specification.

The Specialty Steel Industry of North America advises keeping paper or other protective wrapping on stainless steel until processing is complete, and asking the manufacturer how long the paper or film can stay in place [4].

The Kaifeng figures quoted below come from its product page for stainless steel interleaving paper.

Cross-section of a steel coil with interleaving paper between the wraps
Between coil wraps the paper has steel on both faces. It keeps the surfaces apart, and it must not add moisture, acidity, soluble salts, dust or loose fibre.

Which properties matter most for each process and finish?

Start from the finish your steel customer ships and the step where the paper goes in, because each application puts a different load on the paper. EN 10088-2 designates cold-rolled finishes by code: 2B is cold rolled, heat treated, pickled and skin passed; 2R is bright annealed and highly reflective; 2J is brushed or dull polished; 2K is a satin polish [1].

Four stainless steel finishes, 2B, 2R, 2J and 2K, shown as surface samples
The four EN 10088-2 cold-rolled finishes. The brighter and more polished the finish, the more smoothness and dust control matter.

Table 1. Where to focus the specification

Process or finish Main risk Specify most carefully
Cold-rolled coil, winding Web breaks under tension Tensile strength MD and CD, basis weight, joints
2B after annealing and pickling Staining, marking pH, chloride, sulphate, moisture
2R (bright annealed) Visible marks on a mirror-like surface Smoothness, dust, lint, chemistry
2J or 2K (brushed, satin) Scratches, fibre on the finish Smoothness of the contact side, dust
Slitting Edge tearing, runnability Tensile and tear strength, roll quality
Cut sheets Sticking, handling Basis weight, stiffness, moisture

This is a framework for the conversation with your steel mill customer or quality team, not a replacement for their specification. Each supplier should name the grade it recommends for each finish, with the reason.

Buying interleaving paper for 2B, 2R or polished stainless?

Send your specification, finish codes, roll sizes and annual tonnage. We price against your coil widths.

Interleaving and industrial papers from Kaifeng

What pH, chloride and sulphate limits should the paper meet?

Use the limits in the steel mill's or end customer's specification: a pH range with lower and upper values, and maximums in mg/kg for water-soluble chloride and sulphate. A limit without a method cannot be checked, so name one for each property.

  • pH of the aqueous extract. ISO 6588-1 measures pH after cold-water extraction [2]; hot extraction is also used, so state which one the result refers to.
  • Water-soluble chloride and sulphate. Name the laboratory method, the extraction and the detection limit for each, and keep the same method for every delivery.

Kaifeng's stainless grade is listed on its product page at pH 7.0 ± 1.0. Chloride and sulphate limits come from the steel customer's specification: write them as maximums with the test method and extraction conditions, and agree whether a certificate of analysis comes with each batch.

PropertypH, aqueous extract
Value7.0
Tolerance± 1.0
MethodISO 6588-1
ExtractionCold or hot?

One line written out in full, using the pH value on the Kaifeng product page. State whether the result refers to cold or hot extraction.

Why steel producers care: the Australian Stainless Steel Development Association notes that when relative humidity exceeds 55%, chlorides can absorb moisture, breaking down the passive film and causing rust spotting [3]. That is why steel customers set a chloride maximum for paper that sits against the steel for weeks.

Moisture

Moisture in the paper ends up next to the metal. Specify a range and keep rolls dry before use. The product page lists moisture of 6.0% ± 2.0.

How does basis weight change cushioning and cost?

Basis weight is usually written in g/m², often shortened to gsm. Heavier grades give more cushioning when you interleave cut sheets and on high-gloss polished surfaces; lighter grades add less bulk to a coil and give more paper per tonne. Agree a basis weight with a tolerance, and add thickness as well, because two papers of the same weight can differ in thickness. The product page lists 25–45 g/m² and 33–60 µm.

Coils

Lighter grades add less bulk to a coil and give more paper per tonne. Winding needs tensile strength in MD and CD.

Cut sheets and polished surfaces

Heavier grades give more cushioning. For cut sheets, also specify stiffness and moisture.

Basis weight also changes what a tonne buys. One tonne of paper covers 1,000,000 ÷ grammage square metres:

Table 2. Paper area and length per tonne, by grammage

Grammage (gsm) Area per tonne Length per tonne at 1,250 mm width
25 g/m² 40,000 m² 32,000 m
30 g/m² 33,333 m² 26,667 m
35 g/m² 28,571 m² 22,857 m
40 g/m² 25,000 m² 20,000 m
45 g/m² 22,222 m² 17,778 m

At the same price per tonne, a 30 g/m² grade costs 25% less per square metre than a 40 g/m² grade. Compare quotes per square metre, then confirm in a line trial that the lighter grade still protects your finish and survives winding. Reel length at a given diameter depends on thickness, so check it against your unwind limits too.

How smooth and dust-free must paper be for 2R and polished finishes?

On high-gloss reflective and polished surfaces, the paper's surface quality decides whether it can protect the finish and the steel ships clean. Specify a minimum smoothness for each side: between coil wraps or stacked sheets, the paper has steel on both faces, so the rougher wire side matters too. The product page lists at least 40 s on the upper side and 15 s on the wire side; Bekk smoothness, ISO 5627, is a common method that reports seconds [2].

SteelInterleaving paperSteelUpper side≥ 40 s on the product pageWire side≥ 15 s · also against steelSet a minimum for each side and name the method, such as Bekk (ISO 5627).
Between coil wraps or stacked sheets both faces of the paper touch steel, so the rougher wire side needs its own smoothness minimum.

Loose fibres and dust show on 2R and polished finishes. The supplier should explain how it controls dust and fibre shedding during paper manufacturing and slitting; inspect trial sheets on your own finish under the same lighting you use for final inspection. Have the pulp and fibre source stated in writing as well.

How much strength does the paper need for winding and slitting?

Enough tensile strength to run without breaks on your recoiler at high line tension, and enough tear strength to slit cleanly on industrial slitting lines. Specify:

  • tensile strength in machine and cross direction;
  • tear resistance, for edges and slitting;
  • burst strength, as a general handling check.

The product page lists tensile MD from ≥ 1.5 to ≥ 3.0 kN/m and CD from ≥ 0.7 to ≥ 1.3 kN/m, tear MD from ≥ 120 to ≥ 215 mN and CD from ≥ 130 to ≥ 230 mN, and burst from ≥ 52 to ≥ 100 kPa. These spans cover the whole grammage range, so none of them is an acceptance value for a single grade; agree the values and tolerances of the grade you buy.

What should the specification sheet include?

Each property needs a value, a tolerance or maximum, and a test method agreed with the supplier. Table 3 uses the product page values as examples and lists commonly used ISO methods [2]; confirm which method the supplier actually runs.

Table 3. Stainless steel interleaving paper specification template

Parameter Example (Kaifeng product page) Tolerance or limit Commonly used method
Basis weight 25–45 g/m² (grade range) Agree per grade ISO 536
Thickness 33–60 µm Agree per grade ISO 534
Moisture 6.0% ± 2.0 ISO 287
pH, aqueous extract 7.0 ± 1.0 ISO 6588-1 (cold) or a hot extraction method
Water-soluble chloride Set by the steel customer Maximum in mg/kg Named method and extraction
Water-soluble sulphate Set by the steel customer Maximum in mg/kg Named method and extraction
Smoothness, upper / wire side ≥ 40 s / ≥ 15 s Minimum per side Bekk, ISO 5627
Tensile MD / CD 1.5–3.0 / 0.7–1.3 kN/m (grade range) Agree per grade ISO 1924-2
Tear MD / CD 120–215 / 130–230 mN (grade range) Agree per grade ISO 1974
Burst 52–100 kPa (grade range) Agree per grade ISO 2758

Add the format and documents:

  • roll width and tolerance, maximum diameter, core size, maximum length, joints allowed per roll and how they are marked;
  • winding direction, especially if the two sides are specified differently;
  • wrapping and palletising;
  • what comes with each delivery (certificate of analysis, batch number, quality records) and how the supplier tells you about raw material or manufacturing changes.
White paper roll on a rewinder
Paper on a rewinder. Agree roll width and tolerance, maximum diameter, core size and the joints allowed per roll in the specification.

Questions to send with your RFQ

  • Which of your grades do you recommend for each of our finishes, and why?
  • What are your chloride and sulphate limits, with the test method and extraction conditions?
  • Are the figures typical values or maximums?
  • Is the pH result from a cold or a hot extract?
  • Which method stands behind the smoothness values?
  • How do you control dust and fibre shedding, and what is the pulp and fibre source?

How do you qualify a new interleaving paper supplier?

Qualify on your own line and finish, not on the data sheet alone: paper quality and performance show up on the steel, not on paper.

  1. Agree the specification, test methods and tolerances in writing.
  2. Run a trial roll and inspect the finish after a realistic storage period.
  3. Check each delivery at goods-in: label and batch, roll dimensions, wet patches or damage, and the certificate of analysis.
  4. Keep a retained sample from each batch for critical finishes, so a staining complaint can be traced to a paper lot.
  5. Agree how changes to raw materials or the manufacturing process will be notified.
  6. Audit the production site, on site or by video, if the finish is critical.

Check certificates against their scope, not just their logo. Kaifeng Paper's ISO 9001 quality management, ISO 14001 and ISO 45001 certificates, for example, cover stainless steel interleaving paper together with tipping base paper and food packaging paper, and not every paper the company sells.

Store rolls in their moisture-resistant packaging, off the floor and away from doors and washing areas, and use them in batch order. To start a trial, send your coil and surface finish details.

Send your coil and surface finish details

To compare an offer against your own limits, send your coil and surface finish details.

  1. Share your specification or your steel customer's limits for pH, chloride, sulphate and moisture.
  2. Tell us the finish codes, roll sizes and annual tonnage.
  3. We price stainless interleaving paper against your coil widths.
Related guideHow to Specify Anti-Rust Paper for Metal Parts and Shipping →

FAQs

What is interleaving paper?

Interleaving paper is a thin industrial paper used to interleave layers of a material that would otherwise scratch, mark or stick to itself, such as stainless steel coils and sheets for appliance, building and automotive parts, aluminium, glass or printing plates. For metals, buyers judge it on chemistry, smoothness and strength. Grades differ by basis weight, whether they are bleached, and how tightly soluble salts are controlled.

Is steel interleaving kraft paper made from virgin fibre?

Not necessarily. "Kraft" names a chemical pulping process, so the word alone does not tell you whether a kraft paper grade is made from virgin pulp, recycled fibre or a blend. For stainless steel, have the fibre source stated in writing, because it affects cleanliness and consistency.

What pH should stainless steel interleaving paper be?

Usually near neutral, within the range your steel customer sets. Write it as a lower and upper limit for the aqueous extract, say whether cold or hot extraction is used, and agree batch results if your customer needs them. A single "neutral" claim without a number or method cannot be checked at goods-in.

What chloride level is acceptable in interleaving paper?

There is no universal figure. The steel producer's specification sets it, depending on grade, finish and storage time. Write it as a maximum in mg/kg of water-soluble chloride and tie it to a named test method. Specify sulphate on the same basis, since the two are usually specified together.

Can interleaving paper be reused?

Clean, dry, undamaged paper can sometimes go round again on less critical work. On bright or polished finishes, reused paper risks carrying dust, oil or creases back onto the steel. If you reuse it, set a rule for inspecting and grading it first.

Paper or PE film for stainless steel coils?

Both are used in coil packaging. Paper separates metal surfaces and can take up small amounts of oil; film is chosen where the customer specifies a protective layer on the finished surface. Follow your end customer's specification, and trial any switch on your own line and in your own storage conditions.

Can the same interleaving paper be used for other metals?

Often the same type of industrial kraft paper is used to interleave aluminium, carbon steel and other metal coils and sheets, but the limits change with the metal and the application. Bright aluminium and other high-gloss finishes need the same smoothness and dust control as polished stainless steel. Plain interleaving paper does not prevent corrosion, so carbon steel parts that need protection in a closed pack may call for a VCI paper instead. Write a specific specification for each metal rather than one paper for every application.

How long can interleaving paper stay on stainless steel?

There is no fixed limit. It depends on the paper, storage humidity and the finish. Industry guidance advises checking with the manufacturer how long paper or film can be left in place, and keeping stored steel dry, because moisture and chlorides together drive spotting on stainless surfaces.

Compliance note: limits for interleaving paper are set by the steel producer's or end customer's specification. Parameters quoted from Kaifeng product pages are subject to Kaifeng's current specification sheets and test reports.

Sources

  1. Euro Inox. "Guide to Stainless Steel Finishes" (Building Series, Vol. 1, 3rd edition). Euro Inox, 2005. https://www.edelstahl-rostfrei.de/fileadmin/user_upload/ISER/downloads/Finishes02_EN.pdf Accessed Nov 2026.
  2. Cepi-CTS. "Handbook 5:1 List of properties for which samples are provided and their indicative ranges" (Rev. 45). Cepi, 2026. https://www.cepi.org/wp-content/uploads/2026/05/HB51-Properties-list.pdf Accessed Nov 2026.
  3. Australian Stainless Steel Development Association (L. Pilcher). "Storage and handling of stainless steel". ASSDA, 2024. https://www.assda.asn.au/blog/370-storage-and-handling-of-stainless-steel Accessed Nov 2026.
  4. Specialty Steel Industry of North America. "Care and use in shop". SSINA, n.d. https://www.ssina.com/education/fabrication/care-and-use-in-shop/ Accessed Nov 2026.